Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® A3EG3 - PA66-GF15 - BASF

Material Data Center offers the following functions for Ultramid® A3EG3:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ultramid A datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Características de processamento/físicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 70 / * cm³/10min ISO 1133
Temperatura 275 / * °C -
Carga 5 / * kg -
ASTM Dados
Contração após a moldagem, paralelo 0.0055 mm/mm ASTM D 955
Propriedades mecânicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 6000 / 4500 MPa ISO 527
Tensão no escoamento 130 / 85 MPa ISO 527
Deformação nominal na ruptura 3 / 10 % ISO 527
Módulo de flexão, 23°C 5500 / 4000 MPa ISO 178
Módulo de tensão de fluência, 1000h * / 2500 MPa ISO 899-1
Resistência ao impacto Charpy, +23°C 45 / 70 kJ/m² ISO 179/1eU
Resistência ao impacto Charpy, -30°C 43 / - kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C 8 / 11 kJ/m² ISO 179/1eA
Res. impacto Charpy c/entalhe, -30°C 7 / - kJ/m² ISO 179/1eA
Impacto Izod com entalhe, +23°C 5.5 / 6.5 kJ/m² ISO 180/1A
Ball indentation hardness 200 / 150 MPa ISO 2039-1
ASTM Dados
Resistência à tração na ruptura 114 / - MPa ASTM D 638
Deformação na ruptura 3 / - % ASTM D 638
Módulo de flexão 5170 / - MPa ASTM D 790
Impacto Izod com entalhe, 1/8 in 59 / - J/m ASTM D 256
Impacto Izod com entalhe, baixa temperatura 53 / - J/m ASTM D 256
Temperatura -40 °C -
Propriedades térmicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 260 / * °C ISO 11357-1/-3
Temperatura de deflexão térmica, 1.80 MPa 250 / * °C ISO 75-1/-2
Temperatura de deflexão térmica , 0.45 MPa 250 / * °C ISO 75-1/-2
Coef. de expansão térmica linear, paralelo 32 / * E-6/K ISO 11359-1/-2
Coef. de expansão térmica linear, perpend. 75 / * E-6/K ISO 11359-1/-2
Flamabilidade a 1.5mm esp. nom. HB / * class IEC 60695-11-10
Espessuras do tubo de teste 1.6 / * mm -
ASTM Dados
DTUL @ 66 psi 250 °C ASTM D 648
DTUL @ 264 psi 250 °C ASTM D 648
Temperatura de fusão 260 °C ASTM D 3418
Propriedades elétricasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Constante dielétrica, 1MHz 3.5 / 5.5 - IEC 62631-2-1
Fator de dissipação dielétrica, 1MHz 140 / 1600 E-4 IEC 62631-2-1
Resistividade volumétrica específica 1E13 / 1E10 Ohm*m IEC 62631-3-1
Resistividade superficial específica * / 1E10 Ohm IEC 62631-3-2
Índice comparativo de linha de fuga 550 / - - IEC 60112
ASTM Dados
Resistividade volumétrica específica 1E13 / - Ohm*cm ASTM D 257
Outras propriedadesSeco / CondUnidadeMétodo de ensaio
Absorção de água 7 / * % Sim. to ISO 62
Absorção de umidade 2.2 / * % Sim. to ISO 62
Densidade 1230 / - kg/m³ ISO 1183
Absorção de água, equilíbrio 7 % ASTM D 570
Densidade 1240 kg/m³ ASTM D 792
Propriedades específicas do materialSeco / CondUnidadeMétodo de ensaio
ISO Dados
Índice de viscosidade 145 / * cm³/g ISO 307, 1157, 1628
Características
Processamento
Moldagem por injeção, Outros tipos de extrusão
Forma de entrega
Granulos, Cor natural
Aplicaciones
Automóvel, Elétrica e Eletrônica
Disponibilidade regional
América do Norte, Ásia Pacífico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.